Abstract: PZT nano-crystalline powders were prepared by sol-gel process.Zirconium oxynitrate, tetrabutyl titanate and lead acetate were used as raw materials and ethylene glycol as solvent.
摘 要: 以硝酸氧锆、 钛酸四丁酯、 醋酸铅为原料, 乙二醇为溶剂, 用溶胶-凝胶技术制备了钛矿型的锆钛酸铅(PZT)纳米晶。