The purity 99.99% of scandium oxide(Sc 2O 3) was prepared from tungstenic slag with extraction process.
用萃取法从钨矿渣制得纯度为99.99%的。
The purity 99.99% of scandium oxide(Sc 2O 3) was prepared from tungstenic slag with extraction process.
用萃取法从钨矿渣制得纯度为99.99%的。
In order to recover the tungstenic dust, sodium carbonate was added to it and smelting test was carried out in a 0. 1MVA electric arc furnace.
要为回收钨尘,利用钨尘灰与碳酸钠在0.1MVA电内进行了回收试验,制成粗钨酸钠。